This study presents the effect of calcined hard kaolin (CHK) as replacement (15–50 wt.%) to Portland cement (PC) on the strength development of cemented paste backfill (CPB) of fine tailings containing sulphide. PC is used as binder at 20 wt.% dosage. The results show that CPB sample containing 30 wt.% CHK replacements produces the desired strength and durability (i.e., 26.1% increase in strength over the curing period between 28 d and 360 d). CPB without CHK does not produce the desired strength and durability (i.e., 32.8% losses in strength over the curing period between 90 d and 360 d). The quantity of expansive gypsum of CPB containing 30 wt.% CHK is obviously less than that of CPB without CHK. The porosity of the fine pore for pore diameter